Characteristics – applications:
- DMn-250 is the electrode having high Mn content. High deposition coefficient and abrasion resistance.
- Suitable for welding the abraded details having hardness of 250 HB. After welding, able to process and cut.
Chemical composition (%):
C | Mn | Si | P | S | |
Required | Not required | ≤ 0.03 | ≤ 0.03 | ||
Obtained | – | – | – | 0.025 | 0.020 |
Mechanical property of weld metal:
Hardness (HB) | |
Obtained | 250-280 |
Instructions for use:
- Clean oil, grease and dust before welding
- Dry the electrode at 200 ~350 0 C for 30 ~60 minutes before welding
- Keep arc as soon as possible
- Process welding edges as regulated
- Select appropriate welding current to avoid possible defects
- Use direct current – positive electrode for welding (DC+)
- Size of the electrode and used current:
Diameter (mm) | Φ 3.2 | Φ 4.0 | Φ 5.0 |
Length (mm) | 350 | 400 | 400 |
Amperage (A) | 120~140 | 170~200 | 200~240 |